100 1 $aHust, Jerome G.
245 10 $aElectrical resistivity of electrolytic iron, SRM 797, and austenitic stainless steel, SRM 798, from 5 to 280 K.
260 $aWashington :$bNational Bureau of Standards,$c1974.