"Human Salivary Derived Esterase" (HSDE) degrades dental composite resin restorative materials.Results and conclusions. Significantly higher amounts of methacrylic acid (MAA) and Bisphenol-A-bis [2, 3-dihydroxypropyl]-ether (Bis-HPPP) were produced in HSDE than in PBS. 180-day HSDE incubated specimens had a lower fracture toughness (KIci) than the non-incubated group (P<0.05). KIci values of PBS incubated groups were not significantly different from that of the non-incubated group. There was a significant negative correlation between the KIci values and Bis-HPPP production.Hypothesis. HSDE degrades the resin-dentin interface to produce biodegradation by-products in amounts which are negatively correlated with a reduction in the interfacial fracture toughness of the resin-dentin bond.Methods. Mini short-rod specimens (n=10/group), fabricated using composite (Z250) and adhesive system (Scotchbond Multi Purposes), were either not incubated; or incubated in Phosphate-Buffered Saline (PBS) or HSDE media. Degradation products were isolated and specimens were fracture toughness tested following 30, 90 or 180-day incubation periods.
Check nearby libraries
Buy this book

Edition | Availability |
---|---|
1
Effect of salivary esterase on integrity and fracture toughness of resin-dentin interface.
2007
in English
0494274573 9780494274576
|
aaaa
|
Book Details
Edition Notes
Source: Masters Abstracts International, Volume: 45-06, page: 3116.
Thesis (M.Sc.)--University of Toronto, 2007.
Electronic version licensed for access by U. of T. users.
ROBARTS MICROTEXT copy on microfiche.
The Physical Object
Edition Identifiers
Work Identifiers
Community Reviews (0)
January 27, 2010 | Edited by WorkBot | add more information to works |
December 11, 2009 | Created by WorkBot | add works page |